Winged Flat Head Screw
STEEL FASTENER WITHOUT SEALING
Self-drilling screw without sealing made of carbon steel with yellow zinc plating or Ecoseal 10k. It is provided with a high-performance drill for drilling, a flat head for a better finish and a “wing” to chisel the substrate to be fixed, placement and improving the aesthetic finish.
Benefits
Applications
METALIC LINE – WINGED FLAT HEAD SCREW
DESCRIPTION | DRILL BIT |
APPLICATION RANGE (MM) |
COATING | TIGHTENING WRENCH | U.M. | FRACTIONED AMMOUNT PER PACKAGE (PC) | MASTER AMMOUNT PER PACKAGE (PC) |
PB 12 – 14X1.1/2” | TCP2 | 0.89 – 3.56 | YELLOW ZINC PLATED | PHS 3 | CX. | 250 | 2500 |
PB 12 – 14X1.3/4” | TCP3 | 2.79 – 5.35 | YELLOW ZINC PLATED | PHS 3 | CX. | 200 | 2000 |
PB 12 – 14X2.1/4” | TCP3 | 2.79 – 5.35 | YELLOW ZINC PLATED | PHS 3 | CX. | 150 | 1500 |
ECOSEAL 10K | 2000 | ||||||
PB 12 – 14X3.1/4” | TCP4 | 3.68 – 7.92 | YELLOW ZINC PLATED | PHS 3 | CX. | – | 1200 |
PB 1/4 – 20X5” | TCP3 | 2.79 – 6.35 | YELLOW ZINC PLATED | PHS 3 | CX. | – | 500 |
COMPOSITION:
Material: Carbon steel with thermal treatment
FINISHING | LAYER THICKNESS | CORROSION RESISTANCE | |
SALT-SPRAY¹ | KESTERNICH² | ||
YELLOW ZINC PLATED | 5 MICRONS | 96 HOURS | N/A³ |
ECOSEAL 10K | 10 MICRONS | 240 HOURS | 10 CYCLES |
1 – ASTM B117, ABNT NBR 8094 and DIN 50021 Standards (red corrosion)
2 – DIN 50018 Standard (admitting 15% red corrosion on screw head)
3 – The test does not apply to the sample. Duration is less than 1 cycle.
Related Products
Conheça Nossos ProdutosFrequently Asked Questions
The problems of tip burning, can be related to the following situations:
- a) High rotation (tip firing): The high rotation of the equipment can cause high wear on the screw tip, due to the high friction index, thus generating the breakage of the cutting rod of the screw tip.
- b) Screw performs two operations at the same time (tip breaking): If the screw is generating two operations at the same time (e.g.: drilling and fastening), the process may slow down the rotation of the screw at the moment of drilling, generating tip burn.
- c) Extension too long: if the extension is too long, it may decrease the voltage of the screwdriver, generating a decrease in rotation, making the drilling process more difficult, and causing the tip to burn.
- d) Boring holes outside the specification (tip flaring): The screw must pierce the specified range of each tip, according to the Hard Technical Bulletin. Drilling above this range causes the tip to burn out.
SOLUTION
The possible solutions for tip burning are listed in the following alternatives:
- a) Use the appropriate equipment, according to Hard specification, of maximum rotation of 2500 RPM and 15Nm of wrench.
- b) During the installation process, the screw should perform one operation at a time, such as:
1º) Drilling;
2º) Laminate;
3º) Screw;
This prevents loss of speed during the process and, consequently, burning of the tip.
- c) Work with extensions of a maximum of 2 meters, preventing loss of tension.
- d) Work according to the drilling range specified in the Hard’s Technical Report, checking the comparative between: TIP TYPE X PURLIN THICKNESS.
Budget for Company
Do you want to buy for CNPJ? Click the button below and speak to one of our experts.
Request a quoteFind a Store
We are present throughout Brazil, click the button below and find the store closest to you.
Find storeBuy Online
You can buy directly from our online store and receive it at your home. More comfort and agility for you.
Go to online store